The devolatilization of a non-coking coal and the reduction of iron oxide fines by volatile matter (VM)were studied non-isothermally using thermogravimetery (TG) in argon atmosphere. Thedevolatilization of the coal showed five different regions in terms of the rate of devolatilization. Themaximum rate of devolatilization and the maximum weight loss occur between 640oC and 725oCfurnace temperature. The effect of the heating rate and the coal particle size on devolatilization werestudied. Increasing the heating rate and the particle size resulted in lower devolatilization. Nonisothermallyreduction of iron oxide by VM in a multi-layered array was investigated. A reductiondegree of 40 percent was reached while heating the pack from room temperature to 950oC.Threedistinct regions of reduction were observed for reduction of Fe2O3. The XRD patterns confirmed thestepwise reduction of iron oxide.

کلیدواژه ها:

Volatile MatterDevolatilizaitonNon-isothermal ReductionIron OxideNon-coking Coal

نویسندگان

M. H Hemmati

Department of Metallurgical Engineering, Iron and Steel Research Center, Ferdowsi University of Mashhad, Iran

j Vahdati Khaki

Department of Metallurgical Engineering, Iron and Steel Research Center, Ferdowsi University of Mashhad, Iran

A Zabett

Department of Metallurgical Engineering, Ferdowsi University of Mashhad, Iran