Processing of Spherical Zirconia Powder in Microemulsion System

سال انتشار: 1385
نوع سند: مقاله کنفرانسی
زبان: انگلیسی
مشاهده: 1,591

فایل این مقاله در 13 صفحه با فرمت PDF قابل دریافت می باشد

استخراج به نرم افزارهای پژوهشی:

لینک ثابت به این مقاله:

شناسه ملی سند علمی:

SCCE06_136

تاریخ نمایه سازی: 18 دی 1385

چکیده مقاله:

The water droplets in the microemulsion system of cyclohexane/water/TritonX-100/hexyl alcohol can act as the nano-reactors which solubilize zirconium oxychloride and ammonia separately. The precipitation reactions will take place in the confined spaces determined by the droplets size. The minute original reactors help us obtain nano-size spherical zirconia amorphous powder with uniform diameter distribution and weak aggregate. Such powder begins to crystallize at the temperature about 475°C, and its shrinkage of densification will be The powder is formed by dry pressing process. elementarily finished from 1080 to 1280°C.‍ The 99% relative density and 100% tetragonal phase can be btained when the green body is sintered at 1400° C for 2 h.

نویسندگان

مهدی درگاهی

Undergraduate student, School of Chemical Engineering, University of Kashan

سحر شیوایی

Undergraduate student, School of Chemical Engineering, University of Kashan