EFFECT OF COMPRESSION, PRE-HEATING TEMPERATURE AND BORON ADDITION ON THE PRODUCTION OF NANO-STRUCTURED NIAL INTERMETALLC COMPOUND COMBUSTION SYNTHESIS
سال انتشار: 1390
نوع سند: مقاله کنفرانسی
زبان: انگلیسی
مشاهده: 323
فایل این مقاله در 8 صفحه با فرمت PDF قابل دریافت می باشد
- صدور گواهی نمایه سازی
- من نویسنده این مقاله هستم
استخراج به نرم افزارهای پژوهشی:
شناسه ملی سند علمی:
UFGNSM03_122
تاریخ نمایه سازی: 10 تیر 1396
چکیده مقاله:
NiAl intermetallic compounds have special properties that make them a suitable material for high temperature structural applications. Recently, production of these materials by self-propagating hightemperature synthesis (SHS) within a short time of processing and low energy consume has attracted scientist s attention. In this research, the effect of parameters such as pre-heat temperature, the amount of compression, and boron additions on the process has been analyzed. Ni3Al(B) was produced by mixing of elemental powder of nickel and aluminum in a 3:1 ratio with different amount of boron in a ball mill, compression of the mixture and combustion synthesis in an argon protected atmosphere. Structural changes induced by different parameters were tracked by X-ray diffractometery and scanning electron microscopy.
کلیدواژه ها:
نویسندگان
FARAHNAZ HAFTLANG
Ms, Materials Engineering and Industry Department Semnan University, Semnan, Iran, ۳۵۱۹۶۳۷۵۸۹
SINA SANJARI
Ms, Materials Engineering and Industry Department Semnan University, Seттап, Iraп, ۳۵۱۹۶۳۷۵۸۹